TY - JOUR
T1 - Investigation of the use of extended surfaces in paraffin wax phase change material in thermal management of a cylindrical lithium-ion battery
T2 - Applicable in the aerospace industry
AU - Chen, Haiji
AU - Abidi, Awatef
AU - Hussein, Ahmed Kadhim
AU - Younis, Obai
AU - Degani, Mohamed
AU - Heidarshenas, Behzad
N1 - Publisher Copyright:
© 2021 Elsevier Ltd
PY - 2022/1
Y1 - 2022/1
N2 - The use of phase change materials (PCMs) for cooling lithium-ion batteries is examined in this research. Because of the unique benefits of lithium-ion batteries, their use in electric cars has gotten a lot of attention. The lithium-ion battery is one of the most extensively utilized components as the heart of a hybrid car. These batteries generate a lot of heat while charging or discharging. If the batteries are not correctly handled, their life will be drastically shortened. In this study, a cylindrical battery is submerged in a PCM-filled chamber. Several fins of the same length are placed on the battery. The aim is to find the ideal battery compartment size and fin count to lower maximum battery temperature during the discharging process. COMSOL Multiphysics commercial software is used for the simulations. The results show that the battery with 15 fins has the best PCM melting performance at the beginning of cooling process. After one third of the cooling time, the maximum melting of PCM that is equal to 26.159% takes place. Also, in the entire cooling process, the lowest maximum temperature and the maximum volume fraction of the liquid occur when the number of fins is 9. The battery temperature rises as the number of fins increases beyond nine. Furthermore, an enclosure with the lowest maximum temperature is supplied to enclosure the lithium-ion battery.
AB - The use of phase change materials (PCMs) for cooling lithium-ion batteries is examined in this research. Because of the unique benefits of lithium-ion batteries, their use in electric cars has gotten a lot of attention. The lithium-ion battery is one of the most extensively utilized components as the heart of a hybrid car. These batteries generate a lot of heat while charging or discharging. If the batteries are not correctly handled, their life will be drastically shortened. In this study, a cylindrical battery is submerged in a PCM-filled chamber. Several fins of the same length are placed on the battery. The aim is to find the ideal battery compartment size and fin count to lower maximum battery temperature during the discharging process. COMSOL Multiphysics commercial software is used for the simulations. The results show that the battery with 15 fins has the best PCM melting performance at the beginning of cooling process. After one third of the cooling time, the maximum melting of PCM that is equal to 26.159% takes place. Also, in the entire cooling process, the lowest maximum temperature and the maximum volume fraction of the liquid occur when the number of fins is 9. The battery temperature rises as the number of fins increases beyond nine. Furthermore, an enclosure with the lowest maximum temperature is supplied to enclosure the lithium-ion battery.
KW - Cooling
KW - Fin
KW - Li-ion battery
KW - PCM
KW - Thermal management
UR - http://www.scopus.com/inward/record.url?scp=85120816848&partnerID=8YFLogxK
U2 - 10.1016/j.est.2021.103685
DO - 10.1016/j.est.2021.103685
M3 - Article
AN - SCOPUS:85120816848
SN - 2352-152X
VL - 45
JO - Journal of Energy Storage
JF - Journal of Energy Storage
M1 - 103685
ER -