TY - JOUR
T1 - Different cavity disinfectant efficacy against S.mutans and shear bond strength of caries affected dentin bonded to resin restoration
AU - AlSheikh, Rasha
AU - Abduldaiem, Omar Yousif
AU - Alkhalifa, Muneera S.
AU - Jillani, Mona Shah
AU - Dehailan, Laila Al
AU - Barakat, Ali
AU - Alazmah, Abdulfatah
AU - Hameed, Mohammad Shahul
AU - Niazi, Fayez
N1 - Publisher Copyright:
© 2023
PY - 2023/6
Y1 - 2023/6
N2 - Aims: The existing study aimed to assess the survival rate of S.mutans and shear bond strength (SBS) of resin adhesive restoration bonded to carious affected dentin (CAD) after using different cavity disinfectants (Chitosan, Fotoenticine®, and CO2 laser) in comparison to Chlorhexidine (CHX). Materials and methods: The study included human mandibular molars assessed on International Caries Detection and Assessment System (ICDAS) score 4 and 5. The cusp part of the clinical crown was cut off until the reduction reaches the central fossa while being continuously supplied with water coolant till the tooth cementoenamel junction (CEJ). The root sections were embedded in polymethyl methacrylate acrylic resin followed by culturing S.mutans biofilm on the CAD surface. Specimens were arbitrarily allocated into four groups(n = 10) based on the type of disinfection. Group 1 (2% CHX), Group 2 (Chitosan), Group 3 (Fotoenticine), and Group 4 (CO2 laser). S.mutans survival rate was assessed and CAD was restored with a composite restorative material. Thermoocycling of the samples was performed and a universal testing machine (UTM) and Stereomicroscope were used to identify bond integrity and type of fracture. ANOVA and Tukey multiple comparison tests were used to assess SBS. Data on the survival rate of S. mutans were compared between groups using the nonparametric Kruskal-Wallis test Results: Outcomes revealed that Group 1 (CHX) displayed the highest survival rate (0.65 ± 0.10). However, lowest survival rate was demonstrated by Group 3 (Fotoenticine) treated specimens (0.25 ± 0.06). It was also discovered that CHX unveiled highest bond strength values (21.48 ± 1.39 MPa). Nevertheless, Group 2 (Chitosan) showed lowest SBS (11.01 ± 1.00 MPa). Intergroup comparison analysis presented that group 1, and group 4 (Co2 laser) (17.76 ± 0.41 MPa) displayed no significant difference in their bond integrity achieved. (p > 0.05). However, group 3 (Fotoenticine) (16.28 ± 0.51 MPa) and group 2 demonstrated comparable outcomes of SBS. (p > 0.05) Conclusion: The use of CHX and CO2 lasers as disinfectants on the CAD surface resulted in a positive impact on the SBS of resin composite, according to the study's findings. However, it is worth noting that Fotoenticine exhibited better antimicrobial efficacy against S.
AB - Aims: The existing study aimed to assess the survival rate of S.mutans and shear bond strength (SBS) of resin adhesive restoration bonded to carious affected dentin (CAD) after using different cavity disinfectants (Chitosan, Fotoenticine®, and CO2 laser) in comparison to Chlorhexidine (CHX). Materials and methods: The study included human mandibular molars assessed on International Caries Detection and Assessment System (ICDAS) score 4 and 5. The cusp part of the clinical crown was cut off until the reduction reaches the central fossa while being continuously supplied with water coolant till the tooth cementoenamel junction (CEJ). The root sections were embedded in polymethyl methacrylate acrylic resin followed by culturing S.mutans biofilm on the CAD surface. Specimens were arbitrarily allocated into four groups(n = 10) based on the type of disinfection. Group 1 (2% CHX), Group 2 (Chitosan), Group 3 (Fotoenticine), and Group 4 (CO2 laser). S.mutans survival rate was assessed and CAD was restored with a composite restorative material. Thermoocycling of the samples was performed and a universal testing machine (UTM) and Stereomicroscope were used to identify bond integrity and type of fracture. ANOVA and Tukey multiple comparison tests were used to assess SBS. Data on the survival rate of S. mutans were compared between groups using the nonparametric Kruskal-Wallis test Results: Outcomes revealed that Group 1 (CHX) displayed the highest survival rate (0.65 ± 0.10). However, lowest survival rate was demonstrated by Group 3 (Fotoenticine) treated specimens (0.25 ± 0.06). It was also discovered that CHX unveiled highest bond strength values (21.48 ± 1.39 MPa). Nevertheless, Group 2 (Chitosan) showed lowest SBS (11.01 ± 1.00 MPa). Intergroup comparison analysis presented that group 1, and group 4 (Co2 laser) (17.76 ± 0.41 MPa) displayed no significant difference in their bond integrity achieved. (p > 0.05). However, group 3 (Fotoenticine) (16.28 ± 0.51 MPa) and group 2 demonstrated comparable outcomes of SBS. (p > 0.05) Conclusion: The use of CHX and CO2 lasers as disinfectants on the CAD surface resulted in a positive impact on the SBS of resin composite, according to the study's findings. However, it is worth noting that Fotoenticine exhibited better antimicrobial efficacy against S.
KW - Chitosan
KW - Chlorhexidine
KW - CO2 lasers
KW - Fotoenticine
KW - Photodynamic Therapy
KW - Shear bond strength
UR - http://www.scopus.com/inward/record.url?scp=85160033195&partnerID=8YFLogxK
U2 - 10.1016/j.pdpdt.2023.103560
DO - 10.1016/j.pdpdt.2023.103560
M3 - Article
C2 - 37031900
AN - SCOPUS:85160033195
SN - 1572-1000
VL - 42
JO - Photodiagnosis and Photodynamic Therapy
JF - Photodiagnosis and Photodynamic Therapy
M1 - 103560
ER -