Correction: Repair Bond Strength of Composite Resin to Aged Resin and Glass-Matrix CAD/CAM Ceramic Materials Using Two Different Repair Systems (Coatings, (2021), 11, 1331, 10.3390/coatings11111331)

Sarah Alnafaiy, Nawaf Labban, Ahmed Maawadh, Huda Alshehri, Refal Albaijan

Research output: Contribution to journalComment/debate

Abstract

Incorrect Materials and Methods The authors wishe to make the following corrections to this paper [1]: In the fourth paragraph of the Materials and Methods Section, (1) in the second sentence, replace “2.5 mm thickness” with “2 mm thickness”; (2) in the third sentence, replace “120 s” with “10 s”; (3) in the fourth sentence, delete “, followed by light polymerization for another 15 s”; (4) delete the last two duplicated sentences, “The silicone mold was gently sectioned using a scalpel, and excess composite material was removed, followed by light polymerization for another 15 s. The specimens were then stored in distilled water at room temperature for 24 h before the SBS test.” The authors would like to apologize for any inconvenience caused to the readers by these changes and state that the scientific conclusions are unaffected. The original publication has also been updated.

Original languageEnglish
Article number570
JournalCoatings
Volume12
Issue number5
DOIs
StatePublished - May 2022

Fingerprint

Dive into the research topics of 'Correction: Repair Bond Strength of Composite Resin to Aged Resin and Glass-Matrix CAD/CAM Ceramic Materials Using Two Different Repair Systems (Coatings, (2021), 11, 1331, 10.3390/coatings11111331)'. Together they form a unique fingerprint.

Cite this